PWHT Minimum Material Thickness Application

10/16/2009 3:15 AM

What is the minimum thickness of a material before it can be qualified for PWHT (Post Weld Heat Treatment)?

Reply
Interested in this topic? By joining CR4 you can "subscribe" to
this discussion and receive notification when new comments are added.
Member

Join Date: Oct 2009
Location: Edmonton, Alberta, Canada
Posts: 7
#1

Re: PWHT Minimum Material Thickness Application

10/28/2009 12:48 PM

Please refer to Section VIII Div I , UCS-56 for guidelines regarding PWHT of Carbon Steel.