Carburizing of AISI 1020

03/19/2008 2:06 AM

What is the maxomum hardness we can achieve from Carburizing of AISI 1020 0.8mm strip. quenched in oil, for minimum distortion.

Reply
Interested in this topic? By joining CR4 you can "subscribe" to
this discussion and receive notification when new comments are added.
Power-User
Engineering Fields - Marine Engineering - New Member United Kingdom - Member - New Member Engineering Fields - Mechanical Engineering - New Member

Join Date: Jun 2007
Location: Birmingham UK
Posts: 253
Good Answers: 1
#1

Re: Carburizing of AISI 1020

03/19/2008 7:01 AM
__________________
Reset, Reset
Reply
Associate

Join Date: Feb 2008
Posts: 47
#2

Re: Carburizing of AISI 1020

03/19/2008 7:04 AM

About 55 to 58 rc.