Mechanical Properties U.T.S. -555 N/mm2 El. - 37.50 % (L=4d) what is (L=4d) means in this
That means the gage length of the test specimen is 4x the diameter:
(one) Standard Test Method:
ASTM E8/E8M-08 Standard Test Methods for Tension Testing of Metallic Materials
....."1.2 The gage lengths for most round specimens are required to be 4D for E 8....."