how we make welding procedure

03/06/2012 12:42 PM

we had qualify the procedure for 312 Gr.304L for SMAW process, with that can we make WPS for 312 Gr.316L for same SMAW process, is there any essential variable for that?

Register to Reply
Interested in this topic? By joining CR4 you can "subscribe" to
this discussion and receive notification when new comments are added.
Guru

Join Date: Oct 2008
Posts: 42357
Good Answers: 1695
#1

Re: how we make welding procedure

03/06/2012 2:19 PM
Register to Reply
Power-User
Hobbies - Target Shooting - New Member

Join Date: Feb 2010
Location: Florida
Posts: 259
Good Answers: 29
#2

Re: how we make welding procedure

03/07/2012 8:21 AM

The "essential variable" is the base metal. A change in an essential variable requires a procedure qualification record (PQR).

You can find qualified procedures online. Probably from one of the links lyn provided.

__________________
Si vis pacem, para bellum
Register to Reply
Register to Reply 2 comments

Previous in Forum: Friction Inducing Bearing?   Next in Forum: Fans, Chamber Size & Static Pressure--Co-relationship/How to Control?

Advertisement