PWHT

11/26/2012 7:34 AM

Why code B31.3 told us to perform always PWHT for thickness above 19 MM and is not required for below 19mm unless there is material or client specification reqirement???

Register to Reply
Interested in this topic? By joining CR4 you can "subscribe" to
this discussion and receive notification when new comments are added.
Guru
United Kingdom - Member - Indeterminate Engineering Fields - Control Engineering - New Member

Join Date: Jan 2007
Location: In the bothy, 7 chains down the line from Dodman's Lane level crossing, in the nation formerly known as Great Britain. Kettle's on.
Posts: 32175
Good Answers: 839
#1

Re: PWHT

11/26/2012 7:44 AM

Presumably because B31.3 requires PWHT for 19mm and above regardless of whether there is a client requirement.

__________________
"Did you get my e-mail?" - "The biggest problem in communication is the illusion that it has taken place" - George Bernard Shaw, 1856
Register to Reply
Guru

Join Date: Oct 2007
Location: India
Posts: 1246
Good Answers: 34
#2

Re: PWHT

11/26/2012 10:32 AM

If you know, Why post weld heat treatment is required, then you will know your answer.