Post Forming Heat Treatment of NACT plates

07/25/2010 6:26 AM

Dear all,

Please share views on heat treat ment carried above tempering temperature for NACT plates? one of the case i have come across is stated below.


MOC: SA387 Gr11, Thickness 90mm, Delivery condition: Normalised+accelerated cooled+tempered (NACT)
Contract requirement: Cold formed D''end shall be normalised.
Since plate delivery condition is NACT, Mill certfies plate with 2NACT+3PWHT cycles on simulated coupons.
Fabricator will perform 2nd NACT (Fabricator assures that they do rapid quenching with water and tempering) after cold forming (since normalising is mandatory irrespective % strain)


I am of the view that so far no mill has disclosed how will they perform NACT (complete cycle and cooling rates), thou Simulation is done at mill, in my opinion it is impossible to replicate the same NACT process at fab shop, and can't represent the simulation done at mill.


Also it is not known how mill perform accelerated cooling (by direct water quenching or water sprinklers or forced draft....?)

regads,

inconel

__________________
It is far better to be associated with a few who are right than with the mob which is wrong,because right is always the winner in the end.
Register to Reply
Interested in this topic? By joining CR4 you can "subscribe" to
this discussion and receive notification when new comments are added.
Anonymous Poster
#1

Re: Post Forming Heat Treatment of NACT plates

08/05/2010 3:08 AM

Dear

In my view buyer should ask for these details to mill.These are essential details